7600S Double-beam UV-Vis spectrophotometer
Rapid quantitative elemental analysis
- Measuring range190~1100 nm 波长范围
- Illumination氘灯 + 钨灯组合光源
Spark OES, ICP, UV-Vis
Q/TY spark OES for melt and incoming metal analysis, ICP-OES for trace elements, UV-Vis spectrophotometers and flame photometers for solution quantitation.

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis

Rapid quantitative elemental analysis
Spectrometers & Photometers
Spark OES: a high-voltage spark in argon excites the metal surface; a grating disperses the emission lines onto CCD/PMT arrays, and calibration curves convert intensities into concentrations — 20–30 elements in 10–30 s, ideal for melt control and incoming checks.
ICP-OES: solutions nebulise into an argon plasma (6000–10000 K) for complete atomisation, enabling ppb-level multi-element analysis.
UV-Vis: Beer-Lambert law A = εbc with double-beam referencing for stable baselines (e.g. 7600S).
Flame photometry: alkali metals emit characteristic light in the flame with intensity proportional to concentration — simple and economical for K/Na/Li.
Spectrometers & Photometers
Spectrometers & Photometers
1. Beer-Lambert: A = εbc; with ε=2000 L/(mol·cm), c=2×10⁻⁵ mol/L, b=1 cm, A = 0.040; keep absorbance between 0.1 and 0.8.
2. Calibration: ≥5 points with r² ≥ 0.999; run a mid-check each batch and recalibrate on >5% drift.
3. Detection limit: MDL = 3σ/slope; σ=0.002 Abs and slope 0.05 Abs/(mg/L) give 0.12 mg/L.
4. Type standardisation (OES): correct drift per element ki = Rref/Rmeas with a control sample at the start of each shift.
5. Internal standard: ratio R = Ielement/Imatrix cancels excitation fluctuations.
Spectrometers & Photometers
| Standard | Title | Scope |
|---|---|---|
| GB/T 4336-2016 | Carbon and low-alloy steels by spark OES | Steel quick analysis |
| GB/T 11170-2008 | Stainless steel by spark-discharge OES | Grade judgement |
| GB/T 20975 series | Aluminium alloys by OES | Non-ferrous metals |
| GB/T 9721-2006 | Chemical reagents — UV spectrophotometry | UV-Vis quantitation |
| ISO 11885 | Water quality — ICP-OES for selected elements | Environmental ICP |
Melt-control programs need per-grade control samples each shift; note spark conditions for interstitial elements.
Spectrometers & Photometers
1. Principle follows element and concentration: major and minor elements (0.001–30%) in metal use spark OES; trace levels (ppb to ppm) use ICP; single-element rapid quantification uses spectrophotometry or flame photometry.
2. Three things about OES: channel count and element coverage, detection limits (C/S/P are hardest), argon flush and standardisation. TY-9000 class suits multi-base steel and non-ferrous; Q4/Q8 suit high accuracy and precious metals.
3. Preparation decides data quality: flat, oxide-free, oil-free surfaces with a cutter and grinder; solid standards must match the matrix or matrix effects bias results by more than 10%.
4. ICP does not replace OES: OES is fast (90 s) on solid metal; ICP is slow (2 h preparation) on liquids and traces. Use OES for incoming metal, ICP for water.
5. Spectrophotometer by wavelength: visible (325–1000 nm) for routine colorimetry, UV-Vis (190–1100 nm) for organics and low concentrations, flame photometry for Na/K/Li/Ca.
6. Site and consumables: OES needs 99.999% argon, stable power and a dedicated earth; ICP needs a fume hood and argon; spectrophotometers need dark, stable temperatures.
| Model | Principle | Strength | Typical use |
|---|---|---|---|
| TY-9000 / TY-9610 | Spark OES | Multi-element in steel and non-ferrous | Furnace analysis, incoming checks |
| Q2 / Q4 | Spark OES | Major elements in metals | Foundries, machining |
| Q6 / Q8 | High-accuracy OES | Trace C/S/P, precious metals | Special steel, precious metals |
| ICPE-9000 / ICPS-7510 | ICP-OES | ppb–ppm multi-element | Water, soil, food |
| UV1800 | UV-Vis | Organic and inorganic colorimetry | Chemical, pharma, environment |
| 7600S | Visible | Routine colorimetry | Teaching, routine testing |
| FP640 / FP6410 / 6400A | Flame photometry | Na/K/Li/Ca | Soil, fertiliser, cement |
What keeps data trustworthy: type standardisation with high and low standards every shift, full standardisation monthly, and matrix-matched standards.
Spectrometers & Photometers
Metals: prepare a flat face by lathe or spectral grinder; specimens ≥3 mm thick and ≥φ20 mm, cooled before sparking.
Burn: 5–10 s flush plus 10–20 s analysis; ≥3 burns averaged, RSD >3% triggers investigation (gas, surface, segregation).
Calibration: one- or two-point type standardisation each shift; weekly full-curve checks; retain certificates.
UV-Vis: matched cells (≤0.5%), blank zeroing, absorbance 0.1–0.8.
ICP: complete digestion, on-line internal standard, matrix-matched standards, dilute high-salt samples to protect the nebuliser.
Spectrometers & Photometers

ICPE-9000 plus UV1800 cut Cr(VI), Ni, Cu and Zn testing from three days outsou…

Q4 identifies the grade in 40 seconds and rejected 12 t of stainless tube with…

TY-9000 moves furnace analysis from six minutes in the lab to 90 seconds on th…

An ICPS-7510 auto-samples every 30 minutes for total Cr, Ni and Zn, interlocki…

A TY-9620 at the furnace returns 18 elements in 90 s before tapping, cutting t…

Q8 OES completes 22-element ladle analysis in 40 s with 0.001% carbon detectio…
Our engineers reply within one business day with selection advice, acceptance criteria and lead time.