Straightness restoration of an 8 m roll grinder bed
18 μm → 4 μmFull-length straightness

In an 8 m roll grinder overhaul, bed wear made the ground roll crown unstable and out-of-roundness exceeded 5 μm.

Solution: the MC030-ZJUH5000/0.2 autocollimator (±5000 arcsec range, 0.2 arcsec resolution) measured both planes every 200 mm along the bed; software plotted the error curve with scraping allowances, iterated over three scraping-measurement cycles.

Result: vertical straightness over the full 8 m converged from 18 μm to 4 μm (5 μm horizontally). After reassembly, ground roll roundness stayed within 1.5 μm, meeting factory specification.