The institute had only a 100 kN machine for small specimens; bolts above M24 and 30 mm plate were beyond it, so its CNAS scope-extension application lacked equipment-capability evidence.
Solution: a WES100-300B digital hydraulic universal testing machine, 300 kN class 1, with a stiff six-column frame, flat jaws for plate specimens and V-jaws for rounds. Load, displacement and extension are acquired on three channels, and the extensometer is calibrated to ISO 9513 class 1.
Result: the machine passed JJG 139 verification at class 1; method validation covered M30 bolt tensile and Q355B thick plate, and the uncertainty budgets for Rp0.2 and Rm met CNAS requirements, so the extension passed first time.
Benefit: new business in thick plate and large-bolt testing adds about CNY 600,000 in annual revenue.