Phòng thử nghiệm2025

Mở rộng năng lực thử kéo kim loại

WES100-300B 300 kN cấp 1, hỗ trợ mở rộng CNAS theo GB/T 228.1.

Công ty
Viện kiểm nghiệm độc lập, Tây Nam Trung Quốc
Địa chỉ
Trùng Khánh
Mở rộng năng lực thử kéo kim loại
300 kNDải đo
一次通过Mở rộng CNAS

The institute had only a 100 kN machine for small specimens; bolts above M24 and 30 mm plate were beyond it, so its CNAS scope-extension application lacked equipment-capability evidence.

Solution: a WES100-300B digital hydraulic universal testing machine, 300 kN class 1, with a stiff six-column frame, flat jaws for plate specimens and V-jaws for rounds. Load, displacement and extension are acquired on three channels, and the extensometer is calibrated to ISO 9513 class 1.

Result: the machine passed JJG 139 verification at class 1; method validation covered M30 bolt tensile and Q355B thick plate, and the uncertainty budgets for Rp0.2 and Rm met CNAS requirements, so the extension passed first time.

Benefit: new business in thick plate and large-bolt testing adds about CNY 600,000 in annual revenue.

⇄0So sánhSo sánh thông số