The plant tests M30 grade 10.9 bolts to GB/T 3098.1 for proof load and wedge load. A 600 kN hydraulic press left too little margin, manual valve control made the rate erratic, and elongation scatter across eight pieces reached 3.2%, failing customer re-checks.
Solution: WAW-1000C servo-hydraulic with dedicated tensile fixtures featuring spherical self-alignment and a 6° wedge; the software holds proof load for 15 s automatically and runs the wedge test at a constant 8 mm/min to fracture.
Result: four minutes per piece, 25 minutes for eight instead of 50; scatter down to 1.1% and 100% pass rate on customer re-checks; reports with curves are generated automatically.