Proof load and wedge testing of M30 high-strength bolts

WAW-1000C with dedicated bolt fixtures and automatic rate control runs four minutes per piece, 25 minutes for eight, cutting elongation scatter from 3.2% to 1.1%.

Компания
High-strength bolt maker, Hebei
Адрес
Handan, Hebei
Proof load and wedge testing of M30 high-strength bolts
4 min / 25 minPer piece / batch
3.2% → 1.1%Elongation scatter
100%Re-check pass

The plant tests M30 grade 10.9 bolts to GB/T 3098.1 for proof load and wedge load. A 600 kN hydraulic press left too little margin, manual valve control made the rate erratic, and elongation scatter across eight pieces reached 3.2%, failing customer re-checks.

Solution: WAW-1000C servo-hydraulic with dedicated tensile fixtures featuring spherical self-alignment and a 6° wedge; the software holds proof load for 15 s automatically and runs the wedge test at a constant 8 mm/min to fracture.

Result: four minutes per piece, 25 minutes for eight instead of 50; scatter down to 1.1% and 100% pass rate on customer re-checks; reports with curves are generated automatically.