Chip packaging2025

BGA solder-ball coplanarity and diameter inspection

YR2010S high-magnification vision with coaxial ring light measures 0.3 mm BGA ball coplanarity and diameter, Z repeatability within 1.5 µm, acting as referee for the laser line-scan sorter.

Firma
An IC packaging and test house, E. China
Adresse
Shanghai
BGA solder-ball coplanarity and diameter inspection
≤1.5 μmZ repeatability
3% → 0.4%Scanner false rejects

BGA packages carry 0.3 mm solder balls with a coplanarity limit of 0.08 mm. The laser line-scan sorter produced occasional false rejects, and without a high-magnification referee whole trays were reworked at a loss of thousands of yuan each time.

Solution: a YR2010S vision machine with a long-working-distance objective and coaxial ring light to suppress ball glare. Z auto-focus takes the apex of every ball, then all balls are fitted to a datum plane to output coplanarity and diameter distribution; Z repeatability is within 1.5 µm.

Result: five minutes to re-check one tray, with coplanarity agreeing with the line scanner within 4 µm; the scanner threshold was corrected and false rejects fell from 3% to 0.4%.

Benefit: about 12 trays per month saved from false-reject rework, and the referee data also fine-tunes the ball-attach machine, lifting coplanarity CPK from 1.2 to 1.5.

⇄0VergleichTechnischer Vergleich