Đóng gói chip2025

Đo độ đồng phẳng và đường kính bi hàn BGA

YR2010S đo bi hàn 0,3 mm, lặp lại trục Z ≤1,5 µm.

Công ty
Nhà máy đóng gói kiểm định IC, Đông Trung Quốc
Địa chỉ
Thượng Hải
Danh mục
Máy đo ảnh
Đo độ đồng phẳng và đường kính bi hàn BGA
≤1.5 μmLặp lại trục Z
3% → 0.4%Loại nhầm

BGA packages carry 0.3 mm solder balls with a coplanarity limit of 0.08 mm. The laser line-scan sorter produced occasional false rejects, and without a high-magnification referee whole trays were reworked at a loss of thousands of yuan each time.

Solution: a YR2010S vision machine with a long-working-distance objective and coaxial ring light to suppress ball glare. Z auto-focus takes the apex of every ball, then all balls are fitted to a datum plane to output coplanarity and diameter distribution; Z repeatability is within 1.5 µm.

Result: five minutes to re-check one tray, with coplanarity agreeing with the line scanner within 4 µm; the scanner threshold was corrected and false rejects fell from 3% to 0.4%.

Benefit: about 12 trays per month saved from false-reject rework, and the referee data also fine-tunes the ball-attach machine, lifting coplanarity CPK from 1.2 to 1.5.