Inclusion rating depended on subjective morphology judgement: three inspectors differed by up to 1.5 classes on the same sample, and complaints concentrated on confusion between type B (alumina) and type D (globular) inclusions.
Solution: HX-G5A inverted microscope with dark-field condenser and polariser, built-in ASTM E45 / GB/T 10561 charts, automatic field stitching, aspect-ratio and colour classification giving a suggested A/B/C/D/DS rating for human confirmation.
Result: 96% agreement between inspectors, 25 minutes per sample, within 0.5 class of the steel mill arbitration, and a 40% drop in annual quality claims.