Bearings & special steel2024

Non-metallic inclusion rating to GB/T 10561

Combined dark-field and polarised imaging for A/B/C/D/DS inclusions raised rating consistency from 78% to 96%.

会社名
Bearing steel supplier, Zhejiang
所在地
Hangzhou, Zhejiang
カテゴリ
Microscopes
Non-metallic inclusion rating to GB/T 10561
96%Rating agreement
25 minTime per sample

Inclusion rating depended on subjective morphology judgement: three inspectors differed by up to 1.5 classes on the same sample, and complaints concentrated on confusion between type B (alumina) and type D (globular) inclusions.

Solution: HX-G5A inverted microscope with dark-field condenser and polariser, built-in ASTM E45 / GB/T 10561 charts, automatic field stitching, aspect-ratio and colour classification giving a suggested A/B/C/D/DS rating for human confirmation.

Result: 96% agreement between inspectors, 25 minutes per sample, within 0.5 class of the steel mill arbitration, and a 40% drop in annual quality claims.

⇄0比較仕様比較