Linh kiện thủy lực2022

Y9025B đo độ tròn 0,3 um lõi van servo

Y9025B (0,025 um) kiểm độ tròn 0,3 um, độ trụ 0,6 um lõi van; kẹt van giảm từ 1,2% còn 0,12%.

Công ty
Nhà máy van servo thủy lực, Bắc Trung Quốc
Địa chỉ
Thạch Gia Trang, Hà Bắc
Y9025B đo độ tròn 0,3 um lõi van servo
0.3 μmĐộ tròn lõi van
0.12%Tỷ lệ kẹt

Servo valve spools run in sleeves with 2-3 um clearance; 0.5 um of roundness error can cause sticking. Outsourced metrology took three days, so the shop controlled lapping by feel, and outgoing sticking reached 1.2%.

Solution: a Y9025B roundness tester installed in a shop-floor temperature-controlled corner, with 0.025 um air-spindle accuracy, grading working-edge roundness, cylindricity and coaxiality per GB/T 7235. Five sections per spool, 50 UPR filter, 6 minutes per part.

Results: after match-lapping, spool roundness holds at 0.3 um and cylindricity at 0.6 um, with readings fed back to the lapping machine. Sticking dropped to 0.12%, outsourced metrology was eliminated, saving about 450000 yuan a year.