Chế tạo hàng không2023

CMM Helios-N đo vỏ đường kính 1,2 m

CMM Helios-N đo vỏ 1,2 m quét 5 trục 2400 điểm; kiểm tra giảm từ 16 h còn 3,5 h.

Công ty
Nhà máy vỏ động cơ, Tây Bắc Trung Quốc
Địa chỉ
Tây An, Thiểm Tây
CMM Helios-N đo vỏ đường kính 1,2 m
3.5 hThời gian kiểm
99%Tỷ lệ ghép thành công

The 1.2 m titanium fan casing requires 0.1 mm position on 96 flange holes and 0.05 mm coaxiality on combined datums. Mandrel-and-surface-plate setups took 16 hours per part and covered only a quarter of the holes.

Solution: a Helios-N CMM with 1500 mm travel and a 5-axis scanning head, scanning all flange holes, spigots and coaxial datums at 2400 points per part, with dual-sensor temperature compensation for titanium casing and granite table.

Results: inspection time fell to 3.5 hours with all 96 holes measured, and coaxiality was quantified across full sections for the first time at a stable 0.031-0.044 mm. First-match success at the engine customer rose from 88% to 99%, and inspection manpower was cut by two thirds.

⇄0So sánhSo sánh thông số