Вопросы
Подбор модели · Методика испытаний
Electronic or hydraulic universal testing machine?
Electronic (servo + ball screw) gives precise speed control up to ~300 kN; hydraulic suits high loads to 2000 kN. Under 100 kN, prefer electronic.
How to choose an extensometer?
Clip-on for high accuracy at low cost; video extensometer for high temperature, thin sheets or fragile specimens; automatic for batch testing. Yield strength requires an extensometer.
Does testing speed affect results?
Yes. Most metals are strain-rate sensitive: faster testing raises yield and tensile strength and lowers elongation. Follow ISO 6892-1 method A or B consistently.
Why do grips and alignment matter?
Eccentric loading adds bending, lowering strength and scattering results. Keep alignment within 10% and verify with an alignment fixture periodically.
How often should the machine be calibrated?
Force annually with a 0.05-class proving instrument at 3–5 points; displacement and speed annually; extensometer every two years. Add interim checks with reference specimens.