Станкостроение2025

Угловая вибрация шпинделя на 200 Гц

MC030-ZJHS200-200HZ: спектр угловой вибрации шпинделя при 6000 об/мин.

Компания
Производитель шлифовальных станков, Вост. Китай
Адрес
Шанхай
Угловая вибрация шпинделя на 200 Гц
0.8″ → 0.28″Амплитуда вибрации

A precision cylindrical grinder produced periodic waviness during finish grinding; static tests could not capture the angular vibration of the running spindle.

Solution: the MC030-ZJHS200-200HZ high-speed autocollimator (200 Hz sampling) with a mirror on the spindle nose continuously acquired angular displacement at 6000 r/min, with FFT over 0-100 Hz.

Result: a 12 Hz resonance (0.8 arcsec) was traced to insufficient bearing-seat joint stiffness. After re-preloading and scraping the joint, the peak fell to 0.28 arcsec and workpiece waviness dropped from 0.9 μm to 0.3 μm, meeting precision grade.

⇄0СравнениеСравнение характеристик