Rung góc trục chính ở 200 Hz

MC030-ZJHS200-200HZ ghi phổ rung góc trục ở 6000 vòng/phút.

Công ty
Nhà máy máy mài chính xác, Đông Trung Quốc
Địa chỉ
Thượng Hải
Rung góc trục chính ở 200 Hz
0.8″ → 0.28″Biên độ rung góc

A precision cylindrical grinder produced periodic waviness during finish grinding; static tests could not capture the angular vibration of the running spindle.

Solution: the MC030-ZJHS200-200HZ high-speed autocollimator (200 Hz sampling) with a mirror on the spindle nose continuously acquired angular displacement at 6000 r/min, with FFT over 0-100 Hz.

Result: a 12 Hz resonance (0.8 arcsec) was traced to insufficient bearing-seat joint stiffness. After re-preloading and scraping the joint, the peak fell to 0.28 arcsec and workpiece waviness dropped from 0.9 μm to 0.3 μm, meeting precision grade.