Контроль пищевых продуктов2024

TY-9620 ГФААС для кадмия в рисе

TY-9620 ГФААС по GB 5009.15: Cd в рисе, предел 0,001 мг/кг, расхождение с ICP-MS <5%, 120 образцов в день.

Компания
Центр контроля зерна, Центр. Китай
Адрес
Чанша, Хунань
TY-9620 ГФААС для кадмия в рисе
0.001 mg/kgПредел обнаружения Cd
35 元Стоимость образца

The centre screens incoming rice for cadmium against the 0.2 mg/kg national limit. Everything went to ICP-MS - three days and 200 yuan per sample - while 120 truckloads a day waited at the weighbridge during harvest.

Solution: a TY-9620 graphite-furnace AAS, measuring after microwave digestion per GB 5009.15 with ammonium dihydrogen phosphate as matrix modifier, reaching a 0.001 mg/kg Cd detection limit. Parallel samples in the 0.1-0.4 mg/kg range were benchmarked against ICP-MS.

Results: deviation under 5% with 92-104% spike recoveries. Throughput reached 120 samples a day with 2-hour turnaround, intercepting 100% of over-limit grain; per-sample cost fell to 35 yuan, saving about 780000 yuan in one harvest season.

⇄0СравнениеСравнение характеристик