Free-form cavities of phone mid-frame injection moulds were corrected by bench-worker experience against part warpage, with no quantitative basis. Three correction rounds were typical and delivery took 45 days per mould.

Solution: an ML CMM with a scanning probe samples 3000 points at 2 mm pitch across the cavity; the cloud is best-fitted to CAD and a deviation colour map with ±0.03 mm resolution guides point-by-point correction with amounts read off the map.

Results: correction changed from blind grinding to map-guided work, cutting rounds from three to one and delivery from 45 to 36 days. Final cavity profile reached 0.025 mm with first-shot warpage in spec, saving about 1500 correction hours a year.