Khuôn mẫu2022

CMM ML quét lòng khuôn hướng dẫn sửa

CMM ML quét 3000 điểm lòng khuôn, bản đồ màu ±0,03 mm; sửa khuôn từ 3 vòng còn 1 vòng.

Công ty
Nhà máy khuôn ép, Đông Trung Quốc
Địa chỉ
Côn Sơn, Giang Tô
CMM ML quét lòng khuôn hướng dẫn sửa
3→1Vòng sửa khuôn
0.025 mmBiên dạng lòng khuôn

Free-form cavities of phone mid-frame injection moulds were corrected by bench-worker experience against part warpage, with no quantitative basis. Three correction rounds were typical and delivery took 45 days per mould.

Solution: an ML CMM with a scanning probe samples 3000 points at 2 mm pitch across the cavity; the cloud is best-fitted to CAD and a deviation colour map with ±0.03 mm resolution guides point-by-point correction with amounts read off the map.

Results: correction changed from blind grinding to map-guided work, cutting rounds from three to one and delivery from 45 to 36 days. Final cavity profile reached 0.025 mm with first-shot warpage in spec, saving about 1500 correction hours a year.

⇄0So sánhSo sánh thông số