Machining2024

Incoming grade verification catches 304 supplied as 316

Q4 identifies the grade in 40 seconds and rejected 12 t of stainless tube with 0.02% Mo against a 2.0% minimum, avoiding about CNY 400k in losses.

Компания
Pump and valve manufacturer, Zhejiang
Адрес
Wenzhou, Zhejiang
Incoming grade verification catches 304 supplied as 316
40 sPer spark
12 tRejected lot
约 40 万元Loss avoided

The plant builds chemical pumps with a high share of 316L. Certificates were checked but composition was not, and one corrosion complaint traced back to 304 tube with almost no molybdenum.

Solution: Q4 spark OES, three tubes sampled per incoming batch, two sparks each after grinding, giving Cr/Ni/Mo/C in 40 seconds against the grade specification, with samples retained on failure.

Result: the first verification rejected 12 t of tube sold as 316L (0.02% Mo, 8.1% Ni) and the supplier replaced it in full; with routine incoming spectrometry, material-related complaints fell to zero and annual quality cost dropped about CNY 600k.

⇄0СравнениеСравнение характеристик