Machining2024

Incoming grade verification catches 304 supplied as 316

Q4 identifies the grade in 40 seconds and rejected 12 t of stainless tube with 0.02% Mo against a 2.0% minimum, avoiding about CNY 400k in losses.

Công ty
Pump and valve manufacturer, Zhejiang
Địa chỉ
Wenzhou, Zhejiang
Incoming grade verification catches 304 supplied as 316
40 sPer spark
12 tRejected lot
约 40 万元Loss avoided

The plant builds chemical pumps with a high share of 316L. Certificates were checked but composition was not, and one corrosion complaint traced back to 304 tube with almost no molybdenum.

Solution: Q4 spark OES, three tubes sampled per incoming batch, two sparks each after grinding, giving Cr/Ni/Mo/C in 40 seconds against the grade specification, with samples retained on failure.

Result: the first verification rejected 12 t of tube sold as 316L (0.02% Mo, 8.1% Ni) and the supplier replaced it in full; with routine incoming spectrometry, material-related complaints fell to zero and annual quality cost dropped about CNY 600k.