Construction machinery2024

On-site measurement of an 8 m welded boom with an articulated arm

MC003-SCANARM measures an 8 m boom on site in 90 minutes, replacing a two-day move-to-the-CMM and sectional route.

Компания
Construction machinery plant, Hunan
Адрес
Changsha, Hunan
On-site measurement of an 8 m welded boom with an articulated arm
2 天 → 90 minPer boom
≤0.05 mmRepeatability
0.42 → 0.18 mmDeviation fixed

The boom is 8 m long and 3.2 t; after welding, lug coaxiality (Φ0.3), pin-hole spacing and boom straightness must be checked. The old route craned it to the CMM room and measured in sections over two days, and moving the part could distort it, so the measured state was not the working state.

Solution: MC003-SCANARM with a 4 m arm and laser scanner, measured directly on the fixture with re-positioning on common datum points; lug bores and pin seats are scanned and axes fitted for coaxiality.

Result: 90 minutes per boom with coaxiality repeatability within 0.05 mm; three parts exceeded tolerance at 0.42 mm, traced to uneven shrinkage from the welding sequence and brought to 0.18 mm after re-sequencing, with craning eliminated and safety risk reduced.

⇄0СравнениеСравнение характеристик