Автокомпоненты2023

КИМ Daisy для межосевых размеров картеров КПП

КИМ Daisy с точностью ±(1,9+L/300) мкм контролирует позиционный допуск 0,03 мм отверстий картеров; Cpk вырос с 1,05 до 1,67.

Компания
Завод литья картеров КПП, ЮЗ. Китай
Адрес
Чунцин
КИМ Daisy для межосевых размеров картеров КПП
0.03 mmПозиционный допуск
1.67Cpk позиции

Bearing bores of the transmission housing carry a 0.03 mm position requirement. Indirect checks with mandrels and a roundness tester accumulated conversion errors and could not capture position at all; trial-assembly noise reached 2.8%.

Solution: a Daisy bridge CMM with MPE E=±(1.9+L/300) um and a scanning probe, sampling 3 sections per bore at 120 points each. After fitting the bore-pattern datum frame, position, coaxiality and centre distances are graded per GB/T 1958, with full first-article layout in 40 minutes.

Results: measured bore position of 0.018-0.026 mm with Cpk raised from 1.05 to 1.67. After two die inserts were corrected from the measurement data, trial-assembly noise fell from 2.8% to 0.3%, saving about 600 hours of teardown rework a year.

⇄0СравнениеСравнение характеристик