Двигатели2025

100% контроль HRC фасок клапанов после ТВЧ

HRS-150F: HRC фасок клапанов за 10 с, сортировка 52-56 HRC.

Компания
Завод клапанов ДВС, Вост. Китай
Адрес
Шиянь, Хубэй
Категория
Твердомеры
100% контроль HRC фасок клапанов после ТВЧ
40 → 10 sВремя на клапан
≤0.8 HRCРазброс 3 точек

Engine intake and exhaust valves require 52-56 HRC on the induction-hardened seat cone. A manual Rockwell tester took 40 seconds per valve, so only 2% were sampled; soft valves wore early in service and once triggered a batch claim.

Solution: an HRS-150F motorised Rockwell hardness tester, 98.07 N preliminary and 1471 N total force with a 5 s motorised dwell. A V-locating fixture for the valve stem plus an angle template fixes the indentation position on the cone; upper/lower limits drive automatic grading with audible-visual alarms.

Result: 10 seconds per valve enables 100% inspection with a three-point range within 0.8 HRC; a slow drift from 55.8 to 51.5 HRC caused by hardening-machine power drift was caught on the trend chart one shift early.

Benefit: full inspection replaced sampling with no extra labour, and early valve-wear claims fell to zero that year.

⇄0СравнениеСравнение характеристик