Động cơ2025

Đo HRC toàn phần mặt côn xupap sau tôi

HRS-150F đo HRC mặt côn xupap trong 10 giây, phân loại 52-56 HRC.

Công ty
Nhà máy xupap động cơ, Đông Trung Quốc
Địa chỉ
Thập Yển, Hồ Bắc
Đo HRC toàn phần mặt côn xupap sau tôi
40 → 10 sThời gian/xupap
≤0.8 HRCĐộ lệch 3 điểm

Engine intake and exhaust valves require 52-56 HRC on the induction-hardened seat cone. A manual Rockwell tester took 40 seconds per valve, so only 2% were sampled; soft valves wore early in service and once triggered a batch claim.

Solution: an HRS-150F motorised Rockwell hardness tester, 98.07 N preliminary and 1471 N total force with a 5 s motorised dwell. A V-locating fixture for the valve stem plus an angle template fixes the indentation position on the cone; upper/lower limits drive automatic grading with audible-visual alarms.

Result: 10 seconds per valve enables 100% inspection with a three-point range within 0.8 HRC; a slow drift from 55.8 to 51.5 HRC caused by hardening-machine power drift was caught on the trend chart one shift early.

Benefit: full inspection replaced sampling with no extra labour, and early valve-wear claims fell to zero that year.

⇄0So sánhSo sánh thông số