    제품 개요

    YHRI-150SM传感器数显全洛氏硬度计属于自动型洛氏硬度计,外观新颖,触摸屏幕操作和显示,菜单式结构,采用传感器加载,硬度值以数字直接显示.硬度测试结果可以直接打印输出,
    自动化程度高,消除了操作和读数误差。简便了硬度之间的硬度换算等功能。
    适用于金属材料的洛氏硬度试验。本系列洛氏硬度计操作简便迅速,性能稳定,使用广泛。可进行黑色金属和有色金属的洛氏硬度测定,广泛适用于工厂车间和计量部门。
    二、产品特点:
    1、闭环传感器控制系统,无需砝码;
    2、无需特殊安装,甚至无需售后;
    3、测量精度高;
    4、硬度标尺选择时,提示选用压头;
    5、实验力可定做,结构简单。
    产品型号
    YHRI-150SM
    操作方式
    触摸屏
    加载机构
    高精度传感器加载
    测量标尺
    HRA、HRBW、HRC、HRD、HREW、HRFW、HRGW、HRHW、HRKW、HRLW、HRMW、HRPW、HRRW、HRSW、HRVW、HR15N、HR30N、HR45N、HR15TW、HR30TW、HR45TW、HR15WW、HR30WW、HR45WW、HR15XW、HR30XW、HR45XW、HR15YW、HR30YW、HR45YW
    硬度测量范围
    洛氏:HRA:20 ~ 88,HRB:20 ~ 100,HRC:20 ~ 70表面洛氏:HR15N:70 ~ 91、HR30N:42 ~
    80、HR45N:20 ~ 70、HR15T:73 ~ 93、HR30T:43 ~ 82、HR45T:12 ~ 72
    转换标尺
    HRA、HRB、HRC、HRD、HRF、HBW、HV、HK、HR15N、HR30N、HR45N、HR15T、HR30T、HR45T
    总试验力
    15Kg(147.1N)、30Kg(294.2N)、45Kg(441.3N)、588N(60kgf)、980N(100kgf)、1471N(150kgf)
    执行国家标准
    GB/T230.2 国家标准,JJG112 检定规程
    试验力保持时间 (s)
    3 种试验力保荷满足特殊材料使用。
    初试验力保荷时间
    机器设定 0-60s,最小变动量 1s
    总试验力保荷时间
    机器设定 0-60s,最小变动量 1s
    初试验力返回保荷时间
    机器设定 0-60s,最小变动量 1s
    计算方式
    自动计算
    硬度分辨率
    0.1HR
    试件最大高度
    175mm
    压头中心距离
    160mm
    丝杆直径
    外径 φ40mm
    大平台直径
    φ150mm
    中平台直径
    φ55mm
    V 型台尺寸
    φ35mm
    数据输出
    内置微型打印机
    电源电压
    AC 220V/50Hz
    外形尺寸
    540*215*750mm(长*宽*高)
    净重
    90.5kg
    毛重
    110.5kg

    YHRI-150SM Rockwell Hardness Tester supplied by CHWES. 0 key specifications available on request.

    02

    사양

    * Generated by rule engine over the product database; for pre-selection only.

    03

    측정 원리

    Hardness testing presses an indenter into the surface under a constant load and converts indentation size or depth into a hardness value. Vickers uses a 136° diamond pyramid: HV = 0.1891 × F(N)/d²(mm), where d is the mean diagonal.

    Hot hardness is performed in vacuum or high-purity inert gas. Specimen and indenter are heated independently and must be at the same temperature or corrected per the standard; loading, dwell and unloading all happen inside the hot zone, and the indentation is measured through a high-temperature optic or after cooling. The HMAS series uses a uniform hot zone with ±5 °C uniformity from 200 to 1600 °C.

    • Vickers 0.01–100 kgf: full range, thin layers and case-depth gradients.
    • Rockwell C 150 kgf: fast batch checking of hardened parts.
    • Brinell: castings, annealed and coarse-grain materials.
    • Leeb: portable rebound testing on large parts.
    04

    Process animation

    1. Preparation: polish to Ra ≤ 0.4 µm, remove work-hardened layers.
    2. Mount and align: place the specimen, position the indenter over the test point.
    3. Heat up (hot hardness): evacuate to ≤10⁻² Pa or backfill argon, ramp and soak.
    4. Load: apply force at the set rate, dwell 10–15 s.
    5. Measure: read diagonals or depth, compute HV/HRC.
    6. Gradient: step along depth and plot hardness versus distance.
    0102030405
    05

    Calculation & formulas

    1. Rockwell: HR = K − h/0.002 (K = 100 for HRC, 130 for HRB). At h = 0.078 mm, HRC = 61.

    2. Brinell: HBW = 2F/(πD(D−√(D²−d²))); with F=1838.6 N, D=2.5 mm, d=1.1 mm, HBW ≈ 192.

    3. Vickers: HV = 0.1891·F/d² (F in N); F=9.807 N with d=0.05 mm gives HV ≈ 742.

    4. Test forces: choose Brinell loads by 0.045F/D²; Rockwell 10 kgf preliminary with 60/100/150 kgf total; surface scales 3 / 15/30/45 kgf.

    5. Conversions: HRC ≈ HBW/10 only as a rough mid-range guide — official reports must follow the GB/T 1172 tables.

    06

    규격

    StandardTitleScope
    GB/T 4340.1-2009Vickers hardness test — test methodVickers
    GB/T 230.1-2018Rockwell hardness testRockwell
    GB/T 231.1-2018Brinell hardness testBrinell
    ISO 6507-1Vickers hardness testExport
    ASTM E92Vickers hardness of metallic materialsAmericas
    GB/T 17394.1-2014Leeb hardness testPortable

    Hot hardness has no unified national standard; ASTM E92 practice is normally cited with temperature, atmosphere, dwell and indenter material stated in the report.

    07

    선택 가이드

    1. Principle follows the target: Rockwell for macro hardness and heat-treatment acceptance; Brinell for cast iron, annealed and forged parts where a large indent is representative; Vickers or micro-Vickers for thin layers, coatings and small areas.

    2. Bench or portable: bench units (HRC-150SMJ, HBRVS-187.5) where parts can be brought in; portable Leeb for large moulds, in-service piping and non-removable parts, corrected against a bench reference, typically within ±2 HRC.

    3. One for many: mixed, low-volume shops do well with a Brinell-Vickers-Rockwell combination unit covering HRA/HRB/HRC/HV/HB.

    4. Automation: manual below 100 parts per operator per day; motorised elevation, automatic loading and data upload (HRC-150SMJ) above 200 or for unattended runs.

    5. Reference blocks: two to three blocks covering the working range, checked every shift and sent for annual calibration.

    6. Specimen requirements: Rockwell needs thickness at least ten times the indent depth and Ra ≤1.6 µm; otherwise switch to Vickers or superficial Rockwell.

    ModelPrincipleRangeTypical use
    HRC-150SMJRockwell, motorised digitalHRA/HRB/HRCBatch sampling in heat treatment
    HRC-150SM / HRC-150MRockwellHRA/HRB/HRCIncoming and in-process checks
    HRC-45MSuperficial Rockwell15N/30N/45NSheet, plating, case layers
    HRS-150M / XHRS-150MDigital RockwellHRA/HRB/HRCLines needing data upload
    HBRVS-187.5Brinell-Vickers-RockwellHBW/HRA/HRB/HRC/HVMixed low-volume production

    Three rules for trustworthy data: check the reference block every shift and record it; keep the support face flat and clean; keep indent spacing at least three indent diameters.

    08

    시험 방법

    Specimen. Test and support faces parallel; thickness at least 1.5 × diagonal (Vickers) or 10 × depth (Rockwell); Ra ≤ 0.4 µm, free of scale and oil.

    Room temperature. Select load, apply within 10–15 s, dwell 10–15 s, unload, measure diagonals. Spacing between indentations ≥3d, from the edge ≥2.5d.

    Hot hardness. Load the specimen, evacuate or backfill argon, ramp and soak 20–30 min, lower the indenter, load and dwell, unload, cool or measure hot, then apply the temperature correction.

    Gradient. Step every 0.05–0.1 mm to the hardness plateau; determine effective case depth at 550 HV1 per GB/T 9450.

    Quality control. Check a certified block (e.g. 700 HV1) each shift, recalibrate beyond ±3%, and log furnace curves and atmosphere for hot tests.

    09

    Industry applications

    • Heat-treatment shops: Rockwell HRC sampling of quenched and tempered parts, carburised surface hardness, Brinell HBW on annealed stock.
    • Castings and forgings: body hardness and HAZ values, section hardness gradients indicating cooling rate and structural uniformity.
    • Moulds and tools: HRC versus wear resistance after hardening and tempering, edge-to-core hardness difference on cutting tools.
    • Thin and small parts: case-hardened layers, coatings and sheet need Vickers or superficial Rockwell (HBRVS-187.5 covers HRA/HRB/HRC/HV/HB).
    • Bearings and gears: ring and raceway hardness, case-to-core difference against carburising requirements.
    • Pressure vessels and piping: weld and HAZ hardness to detect brittle microstructures, typically ≤350 HV10.
    • Incoming verification: hardness as the fastest screening method when material grades are mixed, confirmed by OES.
    • Field and in-service: portable Leeb or ultrasonic hardness testers on large immovable parts, corrected against a bench reference.