HOT
MMAS-6 · 2026-11-17 · +86 21 5748 2007
MMAS-6 Metallurgical Microscope (正置透反)
Metallurgical Microscope · 正置透反
- 物镜长距平场消色差物镜(无盖玻片)PL 5X/0.12
- 放大倍数50~600X
- 目镜筒三目镜,倾斜30度,(内置检偏振片,可进行切换)
- 落射照明系统6V 20W卤素灯,亮度可调
By submitting you agree to our privacy policy.
제품 개요
MMAS-6金相显微镜测量分析系统是适用于对不透明物体或透明物体的显微观察。MMAS-6配置落射与透射照明系统、长距平场消色差物镜(无盖玻片)、大视野目镜和内置偏振观察装置,具有图像清晰、衬度好,操作方便等特点,是生物学、金属学、矿物学、精密工程学、电子学等研究的理想仪器。适用于学校、科研、工厂等部门使用。MMAS-6系统配备了研润自主研发的MMAS测量分析系统以及MOS高端光学系统。
一、技术特点:
1、观察系统:铰链式观察镜筒,30度倾斜,单视度可调。WF10X大视野平场目镜,视场范围直径18mm。10X分化目镜,视场范围直径18mm,用于校正中心。
2、机械载物台:双层机械式载物台,尺寸185*140mm;移动范围75*50mm。
3、落射照明系统:6V,20W卤素灯,亮度可调。内置视场光阑、孔径光阑、黄蓝绿以及磨砂玻璃滤色片转换装置,推拉式起偏振器。
4、透射照明系统:内置式6V,20W卤素灯,亮度可调。集光器:带视场光栏集光器;聚光镜:阿贝聚光镜NA1.25,升降上下可调。
5、选配件:
5.1大视野目镜:WF16X(直径11mm);
5.2分划板:10X(直径18mm),格值0.1mm/格;
5.3长距平场消色差物镜(无盖玻璃):PLL20X/0.4、PLL50X/0.7、PLL80X/0.8、PLL100X/0.85(弹簧);
5.4平场消色差物镜(无盖玻璃):PLL100X/1.25(弹簧,油);
5.5转换器:五孔(滚珠内定位);
5.6适配镜:0.4X、0.5X、1X、0.5带0.1mm/格分化尺;
5.7数码摄像机;
5.8滤色片:绿滤色片、黄滤色片;
二、技术参数:
目镜
大视野 WF10X(Φ18mm)
物镜
长距平场消色差物镜(无盖玻片)PL 5X/0.12
长距平场消色差物镜(无盖玻片)PL L10X/0.25
长距平场消色差物镜(无盖玻片)PL L40X/0.60
长距平场消色差物镜(无盖玻片)PL L60X/0.75 (弹簧)
放大倍数
50~600X
目镜筒
三目镜,倾斜30度,(内置检偏振片,可进行切换)
落射照明系统
6V 20W卤素灯,亮度可调
落射照明器带视场光栏、孔径光栏、起偏振片,(黄,蓝,绿)滤色片和磨砂玻璃
调焦机构
粗微动同轴调焦, 微动格值:2μm,粗动松紧可调,带锁紧和限位装置
转换器
四孔(内向式滚珠内定位);选配五孔;
载物台
双层机械移动式(尺寸:185mmX140mm,移动范围:75mmX50mm)
透射照明系统
阿贝聚光镜NA.1.25可上下升降,蓝滤色片和磨砂玻璃,集光器, 卤素灯适用,6V 20W 卤素灯,亮度可调
外形尺寸
435*420*200
配备系统
主机+MMAS数据处理系统1套+MOS光学系统一套+电脑一套
MMAS-6 Metallurgical Microscope (正置透反) supplied by CHWES. 10 key specifications available on request.
사양
| 物镜 | 长距平场消色差物镜(无盖玻片)PL 5X/0.12 |
|---|---|
| 放大倍数 | 50~600X |
| 目镜筒 | 三目镜,倾斜30度,(内置检偏振片,可进行切换) |
| 落射照明系统 | 6V 20W卤素灯,亮度可调 |
| 调焦机构 | 粗微动同轴调焦, 微动格值:2μm,粗动松紧可调,带锁紧和限位装置 |
| 转换器 | 四孔(内向式滚珠内定位);选配五孔; |
| 载物台 | 双层机械移动式(尺寸:185mmX140mm,移动范围:75mmX50mm) |
| 透射照明系统 | 阿贝聚光镜NA.1.25可上下升降,蓝滤色片和磨砂玻璃,集光器, 卤素灯适用,6V 20W 卤素灯,亮度可调 |
| 外形尺寸 | 435*420*200 |
| 配备系统 | 主机+MMAS数据处理系统1套+MOS光学系统一套+电脑一套 |
* Generated by rule engine over the product database; for pre-selection only.
측정 원리
The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.
- Bright field for routine microstructure, inclusions and decarburised layers.
- Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
- Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
- DIC converts tiny height differences into contrast, ideal for polished, unetched samples.
Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.
Process animation
- Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
- Illumination and focus: select BF/DF/POL/DIC and focus.
- Image capture: trinocular port, 1× camera adapter, white balance.
- Scale calibration: calibrate µm per pixel with a stage micrometer.
- Measurement: grain size, case depth, coating thickness, inclusion rating.
Calculation & formulas
1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.
2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.
3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.
4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).
5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.
규격
| Standard | Title | Scope |
|---|---|---|
| GB/T 13298-2015 | Metallic materials — examination of microstructure | Microstructure rating |
| GB/T 6394-2017 | Determination of average grain size | Grain size |
| ASTM E3-11 | Guide for metallographic specimen preparation | Preparation |
| ASTM E112 | Determining average grain size | Grain size |
| ISO 643 | Steels — micrographic determination of grain size | Grain size |
Export projects often require dual GB and ASTM reports; the software ships both rating charts.
선택 가이드
1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.
2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.
3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.
4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.
5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.
6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.
| Series | Type | Typical task | Recommended setup |
|---|---|---|---|
| HX-4A / HX-4B | Upright metallurgical | Routine structure, case depth | 5×/10×/40× + 5 MP camera |
| HX-G2A / G2B | Inverted | Batch samples, no re-mounting | Brightfield + simple polariser |
| HX-G3A | Trinocular inverted | Case depth, rating, reports | Camera + analysis software |
| HX-G4C / G5A | Research inverted | Darkfield/polarised/DIC | Semi-apochromat + motorised stage |
| HX-ZG7 / XSZ-146 | Stereo | Fracture, solder, low-mag locating | Zoom + ring light |
Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.
시험 방법
Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.
Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.
Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.
Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.
Industry applications
- Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
- Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
- Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
- Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
- Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
- Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
- Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
- Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.