Bearing steel2025

Automated inclusion rating of bearing steel to GB/T 10561 method A

HX-G5A with scanning software rates 200 fields in 12 minutes, matching three human inspectors on A/B/C/D classes 96% of the time.

회사명
Bearing-steel tube maker, Henan
주소
Luoyang, Henan
카테고리
Microscopes
Automated inclusion rating of bearing steel to GB/T 10561 method A
12 minPer sample
6 → 30Daily throughput
96%Agreement

Bearing steel demands strict inclusion control; GB/T 10561 method A rates 200 fields. Two inspectors rotated through the work, six samples per person per day, and they disagreed on the B-class (alumina) and D-class (globular) boundaries, generating customer complaints.

Solution: HX-G5A research inverted stand with a motorised stage and the inclusion module. After polishing, one mounting runs the standard grid automatically with autofocus and captures 200 fields, classifying by aspect ratio and morphology into A/B/C/D classes and total rating.

Result: 12 minutes per sample including three minutes of human review; throughput rose from six to thirty samples per day; agreement with three senior inspectors reached 96%, with residual differences on thin B series, and disputes after customer re-checks dropped 70% once the rules were encoded.

⇄0비교사양 비교