HR-150A Rockwell Hardness Tester

Rockwell Hardness Tester

모델HR-150A
  • 洛氏标尺HRA、HRB、HRC、HRD、HRE、HRF、HRG、HRH、HRK
  • 初试验力98.07N (10kgf)
  • 总试验力588N(60kgf),980N(100kgf),1471N(150kgf)
  • 读数方式金属表盘

By submitting you agree to our privacy policy.

01

제품 개요

洛氏硬度计是一种普及型的洛氏硬度测试仪器,适用于金属材料的洛氏硬度试验。本系列洛氏硬度机操作简便迅速,性能稳定,使用广泛。可进行黑色金属和有色金属的洛氏硬度测定,广泛适用于工厂车间和计量部门。
产品特点:
1.金属表盘,稳固、美观、读数正确,采用了成量表盘,品牌质量稳定;
2.铸铁机壳,稳固、耐用、无变形、承受力大;
3.自主加工零件,可替换性高,后续零件供应稳定;
技术参数:
操作方式
手动
洛氏标尺
HRA、HRB、HRC、HRD、HRE、HRF、HRG、HRH、HRK
初试验力
98.07N (10kgf)
总试验力
588N(60kgf),980N(100kgf),1471N(150kgf)
读数方式
金属表盘
硬度分辨率
0.5HR
试件最大高度
170mm
压头中心距离
135mm
数据输出
无
试验力保持时间(S):
人为控制
转换标尺
无
硬度测量范围
HRA:20-88,HRB:20-100,HRC:20-70
执行国家标准
GB/T230.2国家标准,JJG112检定规程
壳体工艺及
铸造壳体
外形尺寸
466×238×630mm
电源
无
重量
65Kg

HR-150A Rockwell Hardness Tester supplied by CHWES. 16 key specifications available on request.

02

사양

洛氏标尺HRA、HRB、HRC、HRD、HRE、HRF、HRG、HRH、HRK
初试验力98.07N (10kgf)
总试验力588N(60kgf),980N(100kgf),1471N(150kgf)
读数方式金属表盘
硬度分辨率0.5HR
试件最大高度170mm
压头中心距离135mm
数据输出无
试验力保持时间(S):人为控制
转换标尺无
硬度测量范围HRA:20-88,HRB:20-100,HRC:20-70
执行国家标准GB/T230.2国家标准,JJG112检定规程
壳体工艺及铸造壳体
外形尺寸466×238×630mm
电源无
重量65Kg

* Generated by rule engine over the product database; for pre-selection only.

03

측정 원리

Hardness testing presses an indenter into the surface under a constant load and converts indentation size or depth into a hardness value. Vickers uses a 136° diamond pyramid: HV = 0.1891 × F(N)/d²(mm), where d is the mean diagonal.

Hot hardness is performed in vacuum or high-purity inert gas. Specimen and indenter are heated independently and must be at the same temperature or corrected per the standard; loading, dwell and unloading all happen inside the hot zone, and the indentation is measured through a high-temperature optic or after cooling. The HMAS series uses a uniform hot zone with ±5 °C uniformity from 200 to 1600 °C.

  • Vickers 0.01–100 kgf: full range, thin layers and case-depth gradients.
  • Rockwell C 150 kgf: fast batch checking of hardened parts.
  • Brinell: castings, annealed and coarse-grain materials.
  • Leeb: portable rebound testing on large parts.
04

Process animation

  1. Preparation: polish to Ra ≤ 0.4 µm, remove work-hardened layers.
  2. Mount and align: place the specimen, position the indenter over the test point.
  3. Heat up (hot hardness): evacuate to ≤10⁻² Pa or backfill argon, ramp and soak.
  4. Load: apply force at the set rate, dwell 10–15 s.
  5. Measure: read diagonals or depth, compute HV/HRC.
  6. Gradient: step along depth and plot hardness versus distance.
0102030405
05

Calculation & formulas

1. Rockwell: HR = K − h/0.002 (K = 100 for HRC, 130 for HRB). At h = 0.078 mm, HRC = 61.

2. Brinell: HBW = 2F/(πD(D−√(D²−d²))); with F=1838.6 N, D=2.5 mm, d=1.1 mm, HBW ≈ 192.

3. Vickers: HV = 0.1891·F/d² (F in N); F=9.807 N with d=0.05 mm gives HV ≈ 742.

4. Test forces: choose Brinell loads by 0.045F/D²; Rockwell 10 kgf preliminary with 60/100/150 kgf total; surface scales 3 / 15/30/45 kgf.

5. Conversions: HRC ≈ HBW/10 only as a rough mid-range guide — official reports must follow the GB/T 1172 tables.

06

규격

StandardTitleScope
GB/T 4340.1-2009Vickers hardness test — test methodVickers
GB/T 230.1-2018Rockwell hardness testRockwell
GB/T 231.1-2018Brinell hardness testBrinell
ISO 6507-1Vickers hardness testExport
ASTM E92Vickers hardness of metallic materialsAmericas
GB/T 17394.1-2014Leeb hardness testPortable

Hot hardness has no unified national standard; ASTM E92 practice is normally cited with temperature, atmosphere, dwell and indenter material stated in the report.

07

선택 가이드

1. Principle follows the target: Rockwell for macro hardness and heat-treatment acceptance; Brinell for cast iron, annealed and forged parts where a large indent is representative; Vickers or micro-Vickers for thin layers, coatings and small areas.

2. Bench or portable: bench units (HRC-150SMJ, HBRVS-187.5) where parts can be brought in; portable Leeb for large moulds, in-service piping and non-removable parts, corrected against a bench reference, typically within ±2 HRC.

3. One for many: mixed, low-volume shops do well with a Brinell-Vickers-Rockwell combination unit covering HRA/HRB/HRC/HV/HB.

4. Automation: manual below 100 parts per operator per day; motorised elevation, automatic loading and data upload (HRC-150SMJ) above 200 or for unattended runs.

5. Reference blocks: two to three blocks covering the working range, checked every shift and sent for annual calibration.

6. Specimen requirements: Rockwell needs thickness at least ten times the indent depth and Ra ≤1.6 µm; otherwise switch to Vickers or superficial Rockwell.

ModelPrincipleRangeTypical use
HRC-150SMJRockwell, motorised digitalHRA/HRB/HRCBatch sampling in heat treatment
HRC-150SM / HRC-150MRockwellHRA/HRB/HRCIncoming and in-process checks
HRC-45MSuperficial Rockwell15N/30N/45NSheet, plating, case layers
HRS-150M / XHRS-150MDigital RockwellHRA/HRB/HRCLines needing data upload
HBRVS-187.5Brinell-Vickers-RockwellHBW/HRA/HRB/HRC/HVMixed low-volume production

Three rules for trustworthy data: check the reference block every shift and record it; keep the support face flat and clean; keep indent spacing at least three indent diameters.

08

시험 방법

Specimen. Test and support faces parallel; thickness at least 1.5 × diagonal (Vickers) or 10 × depth (Rockwell); Ra ≤ 0.4 µm, free of scale and oil.

Room temperature. Select load, apply within 10–15 s, dwell 10–15 s, unload, measure diagonals. Spacing between indentations ≥3d, from the edge ≥2.5d.

Hot hardness. Load the specimen, evacuate or backfill argon, ramp and soak 20–30 min, lower the indenter, load and dwell, unload, cool or measure hot, then apply the temperature correction.

Gradient. Step every 0.05–0.1 mm to the hardness plateau; determine effective case depth at 550 HV1 per GB/T 9450.

Quality control. Check a certified block (e.g. 700 HV1) each shift, recalibrate beyond ±3%, and log furnace curves and atmosphere for hot tests.

09

Industry applications

  • Heat-treatment shops: Rockwell HRC sampling of quenched and tempered parts, carburised surface hardness, Brinell HBW on annealed stock.
  • Castings and forgings: body hardness and HAZ values, section hardness gradients indicating cooling rate and structural uniformity.
  • Moulds and tools: HRC versus wear resistance after hardening and tempering, edge-to-core hardness difference on cutting tools.
  • Thin and small parts: case-hardened layers, coatings and sheet need Vickers or superficial Rockwell (HBRVS-187.5 covers HRA/HRB/HRC/HV/HB).
  • Bearings and gears: ring and raceway hardness, case-to-core difference against carburising requirements.
  • Pressure vessels and piping: weld and HAZ hardness to detect brittle microstructures, typically ≤350 HV10.
  • Incoming verification: hardness as the fastest screening method when material grades are mixed, confirmed by OES.
  • Field and in-service: portable Leeb or ultrasonic hardness testers on large immovable parts, corrected against a bench reference.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0비교사양 비교