FM-200 Metallurgical Microscope (无限远、四色)

Metallurgical Microscope · 无限远、四色

모델FM-200
  • 光学放大倍数100~400X
  • 目镜大视野 WF10X(Φ22mm)、对中望远镜;20X/0.4\8.;40X/0.6\3.5;无限远平场消色差相衬物镜PLL/PHP2(盖玻片厚度1.2mm):10X/0.25\工作距离4.
  • 目镜筒三目镜,倾斜45度,可100%通光投影,瞳距53~75mm
  • 透射照明6V30W卤素灯,亮度可调;转盘式相衬聚光镜,工作距离55mm

By submitting you agree to our privacy policy.

01

제품 개요

FM-200倒置无限远相衬落射荧光显微镜由落射荧光显微系统与倒置生物显微系统组成,采用优良的无限远光学系统,配置长工作距离平场物镜与大视野目镜。紧凑稳定的高刚性主体,充分体现了显微操作的防振要求。旋转摆入摆出式聚光系统,可对高培养皿或圆筒状烧瓶进行无沾染培养细胞观察。落射荧光显微系统采用模块化设计理念,可以安全、快揵地调整照明系统,切换荧光滤色片组件。产品可应用于细胞组织,透明液态组织的显微观察,也可用于生物制药,医学检测、疾病预防等领域内的荧光显微术观察。
一、技术特点:
1、铰链式双目观察镜筒,镜筒45度倾斜;大视野平场目镜,视场范围22mm;
2、透明的载物台板,物镜转换过程可见;同轴高强度挠性钢丝传动的机械载物台配备三种不同规格的培养皿托架,适用于不同培养皿观察;
3、摆入摆出式旋转的聚光系统,可对高培养皿或圆筒状烧瓶进行无沾染培养细胞观察;
4、一体化照明系统,可对光源进行空间调整;
5、落射荧光观察可根据样品检测选择不同的激发光;
6、后置式摄影接口设计;
二、技术参数:
光学放大倍数:100~400X;
目镜:大视野 WF10X(Φ22mm)、对中望远镜;
无限远平场消色差物镜PLL(盖玻片厚度1.2mm):10X/0.25\工作距离4.3、20X/0.4\8.0、40X/0.6\3.5;
无限远平场消色差相衬物镜PLL/PHP2(盖玻片厚度1.2mm):10X/0.25\工作距离4.3、20X/0.4\8.0、40X/0.6\3.5;
目镜筒:三目镜,倾斜45度,可100%通光投影,瞳距53~75mm;
透射照明:6V30W卤素灯,亮度可调;转盘式相衬聚光镜,工作距离55mm;
滤色片:蓝、绿滤色片、磨砂玻璃;
落射荧光照明:100W高压汞灯、电源箱110V/230V可选;
激发滤色片组:
蓝绿激发滤色片组:蓝激发波长:450~490nm、发射波长:515nm;绿激发波长:495~555nm、发射波长:595nm;
紫外、紫激发滤色片组:紫外激发波长:320~380nm、发射波长:435nm;紫激发波长:380~415nm、发射波长:475nm;
载物台:208*227mm,移动范围77*114mm;
玻璃圆载物台:直径118mm;
转换器:五孔;
标本架:
1、内槽尺寸:86mm(宽)X129.5mm(长),可适配圆形培养皿Ф87.5mm;
2、内槽尺寸:34mm(宽)X77.5mm(长),可适配圆形培养皿Ф68.5mm;
3、内槽尺寸::57mm(宽)X82mm(长);
调焦机构:粗微动同轴,带锁紧和限位装置,微动格值:2μm;
三、选配件:
目镜:10X分划广角目镜(Φ22mm),格值0.1mm/格;
物镜:无限远平场消色差PL5X/0.12\26.1;
转换器:六孔(内向式滚珠内定位);
样本适配器:
1、孔座最大直径50.5mm,中心距离63mm,适配外径50mm培养皿观察;
2、孔座最大35.5mm,适配外径35mm培养皿观察;
3、孔座最大尺寸51.5X74.5mm,适配T25型培养皿观察;
4、孔座最大尺寸66.5X66.5mm,适配66X66mm方形培养皿观察;
5、孔座最大尺寸76.6X26.2mm,适配标准载玻片样品观察;
CCD适配镜:0.4X、0.5X、1X、0.5X带分划尺,格值0.1mm/格;
USB/VIDEO摄影接口;
数码相机接口;

FM-200 Metallurgical Microscope (无限远、四色) supplied by CHWES. 15 key specifications available on request.

02

사양

光学放大倍数100~400X
目镜大视野 WF10X(Φ22mm)、对中望远镜;20X/0.4\8.;40X/0.6\3.5;无限远平场消色差相衬物镜PLL/PHP2(盖玻片厚度1.2mm):10X/0.25\工作距离4.
目镜筒三目镜,倾斜45度,可100%通光投影,瞳距53~75mm
透射照明6V30W卤素灯,亮度可调;转盘式相衬聚光镜,工作距离55mm
滤色片蓝、绿滤色片、磨砂玻璃
落射荧光照明100W高压汞灯、电源箱110V/230V可选
蓝绿激发滤色片组蓝激发波长:450~490nm、发射波长:515nm
绿激发波长495~555nm、发射波长:595nm
紫外、紫激发滤色片组紫外激发波长:320~380nm、发射波长:435nm
紫激发波长380~415nm、发射波长:475nm
载物台208*227mm,移动范围77*114mm
玻璃圆载物台直径118mm
转换器五孔
内槽尺寸86mm(宽)X129.5mm(长),可适配圆形培养皿Ф87.5mm
调焦机构粗微动同轴,带锁紧和限位装置,微动格值:2μm

* Generated by rule engine over the product database; for pre-selection only.

03

측정 원리

The metallurgical microscope uses an infinity-corrected optical path with reflected Köhler illumination. Light passes the collector, field stop and aperture stop, is deflected by a semi-transparent mirror through the objective onto the specimen, and returns through the same objective to the eyepiece or camera.

  • Bright field for routine microstructure, inclusions and decarburised layers.
  • Dark field collects scattered light to reveal grain boundaries, cracks and non-metallic inclusions.
  • Polarised light identifies anisotropic phases, spheroidised structures and coating stress.
  • DIC converts tiny height differences into contrast, ideal for polished, unetched samples.

Objectives of 5× to 100× are combined with 10× eyepieces. Higher numerical aperture gives better resolution but shallower depth of field.

04

Process animation

  1. Sampling and preparation: sectioning, mounting, grinding, polishing, etching.
  2. Illumination and focus: select BF/DF/POL/DIC and focus.
  3. Image capture: trinocular port, 1× camera adapter, white balance.
  4. Scale calibration: calibrate µm per pixel with a stage micrometer.
  5. Measurement: grain size, case depth, coating thickness, inclusion rating.
0102030405
05

Calculation & formulas

1. System magnification: M = objective × eyepiece × adapter, e.g. 40× / 10× / 1× = 400×.

2. Resolution: d = 0.61λ/NA (λ≈550 nm). A 40× objective with NA 0.65 resolves 0.52 µm; an NA 0.95 dry objective reaches 0.35 µm.

3. Depth of field scales with λ/NA² — higher NA, shallower depth; use low NA for fracture surfaces.

4. Grain size (GB/T 6394): at 100×, grains N per 645 mm² field follow N = 2G−1; counting 128 grains gives G = log2128 + 1 = 8. Intercept method: mean intercept L̄ = line length ÷ intercepts, G = −6.6437 lg L̄ (mm, 100×).

5. Effective case depth: distance to 550 HV1, fitted from a micro-hardness traverse and averaged over three positions.

06

규격

StandardTitleScope
GB/T 13298-2015Metallic materials — examination of microstructureMicrostructure rating
GB/T 6394-2017Determination of average grain sizeGrain size
ASTM E3-11Guide for metallographic specimen preparationPreparation
ASTM E112Determining average grain sizeGrain size
ISO 643Steels — micrographic determination of grain sizeGrain size

Export projects often require dual GB and ASTM reports; the software ships both rating charts.

07

선택 가이드

1. Surface or cross-section: stereo microscopes (HX-ZG7, XSZ) for fracture surfaces, solder joints and coatings; upright or inverted metallurgical microscopes (HX-4, HX-G series) for microstructure, case depth and inclusions.

2. Upright or inverted: upright for small specimens that are flipped often; inverted (HX-G3A/G4C/G5A) for large, heavy parts such as gears, shafts and tube sections that go straight onto the stage without re-mounting.

3. Optics set the ceiling: plan achromats cover routine rating; semi-apochromats or apochromats with a research stand (HX-G5A) are needed for 1000× precipitates and brightfield/darkfield/polarised switching.

4. Three levels of digitalisation: a 5 MP camera for images; camera plus analysis software (grain size, case depth, inclusions, porosity) for automatic rating and reports; motorised stage with scanning and stitching for unattended batches.

5. Do not forget accessories: polariser, darkfield, DIC, and a microhardness interface.

6. Room: an anti-vibration bench at 20±3 °C for research stands; keep preparation and microscopy rooms separate to avoid abrasive dust.

SeriesTypeTypical taskRecommended setup
HX-4A / HX-4BUpright metallurgicalRoutine structure, case depth5×/10×/40× + 5 MP camera
HX-G2A / G2BInvertedBatch samples, no re-mountingBrightfield + simple polariser
HX-G3ATrinocular invertedCase depth, rating, reportsCamera + analysis software
HX-G4C / G5AResearch invertedDarkfield/polarised/DICSemi-apochromat + motorised stage
HX-ZG7 / XSZ-146StereoFracture, solder, low-mag locatingZoom + ring light

Common misconceptions: higher magnification is not better (numerical aperture limits resolution, 100× dry is the practical ceiling); ignoring stage travel so large samples do not fit; buying the stand without software and still rating by eye, which kills repeatability.

08

시험 방법

Preparation. Section perpendicular to the feature of interest. Keep hot-mounting below 150 °C for aluminium and quenched parts, or use cold mounting. Grind 320→600→800→1200, removing previous scratches at each step; polish with 3 µm then 1 µm diamond. Etchants: 4% nital for carbon steel (3–8 s), aqua regia or electrolytic for stainless, Keller for aluminium.

Examination. Locate a representative field at 5×/10×, then switch to higher power. Rate grain size to GB/T 6394 by comparison or intercept. Measure case depth at 500× with an ocular scale or calibrated software, averaging five readings.

Calibration. Verify µm/pixel daily with a stage micrometer, check against a certified specimen quarterly, record three fields per sample and archive images with scale bars.

Pitfalls. Over-etching widens boundaries and fakes decarburisation; residual scratches can be mistaken for cracks; rounded mounting edges inflate case depth. Keep an unetched specimen for coating and crack review.

09

Industry applications

  • Steel and heat treatment: decarburised depth, carburised/nitrided case depth, grain size (GB/T 6394), non-metallic inclusions (GB/T 10561), banding and Widmanstätten rating.
  • Non-ferrous metals: aluminium grain and recrystallisation, alpha/beta ratio in brass, twinning and corrosion morphology in magnesium.
  • Welding and brazing: penetration, HAZ width, porosity and cracks, intermetallic thickness at dissimilar joints.
  • Additive manufacturing: porosity, lack-of-fusion defects, melt-pool morphology in SLM parts, porosity repeatability within 0.2%.
  • Bearings and gears: martensite rating, retained austenite, carbide network and banding, grinding burn and white layer.
  • Electronics: IMC thickness, plating cross-sections, PCB micro-sections, gold wire ball bonds (stereo plus metallurgical).
  • Powders and ceramics: particle morphology and size, sintered porosity, coating cross-section thickness.
  • Failure analysis: fracture surface macro and micro morphology, corrosion products, crack path and origin, with stereo microscopy for low-magnification locating.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0비교사양 비교