UG CMM for Semiconductor Vacuum Chamber Seal Faces

UG CMM verifies flatness and flange hole positions on 800 mm aluminium vacuum chambers; seal-face flatness holds at 8 um, and first-pass helium leak test rose from 91% to 99.2%.

회사명
A semiconductor equipment chamber maker, E. China
주소
Wuxi, Jiangsu
UG CMM for Semiconductor Vacuum Chamber Seal Faces
8 μmSeal-face flatness
99.2%He leak first-pass

Etch-equipment vacuum chambers have an 800 mm seal face with a 0.01 mm flatness requirement. Straightedge-and-feeler checks were qualitative and missed local dents; first-pass helium leak rate stood at 91% and rework lapping took two days.

Solution: a UG CMM samples the seal face on a 20x20 grid of 400 points together with flange holes and dowel bores. Software grades flatness by the minimum-zone method and outputs a colour map of local highs and lows for selective relapping.

Results: flatness holds at a stable 6-8 um. With dent position and depth quantified, rework changed from full-face lapping to spot correction, cutting rework per chamber from two days to four hours, while first-pass helium leak rate rose to 99.2%.