Stamping2024

In-line 100% inspection of shielding cans at 0.8 s per part

YR-MV1080 dedicated vision with rotary feeding inspects at 0.8 s per part with a 0.02% escape rate, replacing four visual inspectors.

회사명
Precision stamping plant, Guangdong
주소
Dongguan, Guangdong
In-line 100% inspection of shielding cans at 0.8 s per part
0.8 s/件Cycle time
0.02%Escape rate
-4 人Labour

Shielding cans run at eight million pieces a month. Four inspectors watched the conveyor for burrs, dents and dimensions, each handling 8000 parts per day at the edge of fatigue, and escapes reached customers.

Solution: a YR-MV1080 dedicated vision machine with rotary singulation, top and bottom cameras, backlight for the outline and coaxial light for surface scratches; the recipe checks dimensions, hole positions, burr height and dent area, and a nozzle blows rejects into a bin.

Result: 0.8 s per part, matching the 75 ppm line; escape rate 0.02% and false-reject 0.3% falling to 0.05% after lighting tuning; four inspectors moved to packing and sampling, saving roughly CNY 320k a year.

⇄0비교사양 비교