Shielding cans run at eight million pieces a month. Four inspectors watched the conveyor for burrs, dents and dimensions, each handling 8000 parts per day at the edge of fatigue, and escapes reached customers.
Solution: a YR-MV1080 dedicated vision machine with rotary singulation, top and bottom cameras, backlight for the outline and coaxial light for surface scratches; the recipe checks dimensions, hole positions, burr height and dent area, and a nozzle blows rejects into a bin.
Result: 0.8 s per part, matching the 75 ppm line; escape rate 0.02% and false-reject 0.3% falling to 0.05% after lighting tuning; four inspectors moved to packing and sampling, saving roughly CNY 320k a year.