Composites2025

MC003-SCANARM On-Site Scanning of Composite Skin Trims

MC003-SCANARM laser arm scans CFRP skin trim lines in the curing room, reconstructing boundaries at 1.2 M points/s; trim allowance held to ±0.2 mm, replacing templates and cutting skin scrap 65%.

회사명
An aerospace composites plant, E. China
주소
Zhenjiang, Jiangsu
MC003-SCANARM On-Site Scanning of Composite Skin Trims
120 万点/sScan rate
±0.2 mmTrim allowance

After demoulding, CFRP skins were scribed by template and trimmed by hand with ±0.8 mm error; cut-throughs and short edges caused a 4.2% scrap rate on skins worth tens of thousands of yuan each.

Solution: an MC003-SCANARM articulated arm with a laser scanner captures skin surfaces and boundaries at 1.2 million points per second right in the curing room. The cloud is best-fitted to the nominal model and the trim line and hole marks are projected back; the 2.5 m reach covers a full skin.

Results: trim allowance now holds ±0.2 mm, first-pass trim yield rose from 95.8% to 99.7%, and skin scrap fell 65%. Inspection and marking per skin dropped from 90 to 20 minutes, saving about 2.6 million yuan of material a year.