Vật liệu compozit2025

MC003-SCANARM quét mép tấm compozit

Cánh tay MC003-SCANARM quét đường cắt mép tấm sợi carbon 1,2 triệu điểm/s; dung sai ±0,2 mm, phế phẩm giảm 65%.

Công ty
Nhà máy compozit hàng không, Đông Trung Quốc
Địa chỉ
Trấn Giang, Giang Tô
MC003-SCANARM quét mép tấm compozit
120 万点/sTốc độ quét
±0.2 mmDung sai cắt mép

After demoulding, CFRP skins were scribed by template and trimmed by hand with ±0.8 mm error; cut-throughs and short edges caused a 4.2% scrap rate on skins worth tens of thousands of yuan each.

Solution: an MC003-SCANARM articulated arm with a laser scanner captures skin surfaces and boundaries at 1.2 million points per second right in the curing room. The cloud is best-fitted to the nominal model and the trim line and hole marks are projected back; the 2.5 m reach covers a full skin.

Results: trim allowance now holds ±0.2 mm, first-pass trim yield rose from 95.8% to 99.7%, and skin scrap fell 65%. Inspection and marking per skin dropped from 90 to 20 minutes, saving about 2.6 million yuan of material a year.