HXZMP-3000 Auto Grinding-Polishing for Carbide Inserts

HXZMP-3000 prepares six WC-Co inserts per load per ISO 4499, with 100% repeatability of A02B00 porosity ratings; preparation fell from 3 h manual to 45 min, improving eta-phase detection consistency.

회사명
A cemented carbide insert maker, C. China
주소
Zhuzhou, Hunan
HXZMP-3000 Auto Grinding-Polishing for Carbide Inserts
45 minPrep time per batch
100%Rating repeatability

WC-Co inserts are metallographically graded for porosity and eta phase per ISO 4499. Manual preparation took 3 hours per batch, and residual scratch differences between operators swung porosity ratings between A02 and A04 - a customer audit once rejected a lot.

Solution: an HXZMP-3000 automatic grinder-polisher with central force loading six inserts per run, with a locked program of diamond steps 30 um, 6 um, 3 um and 1 um, fixing speed, pressure and time instead of four manual steps.

Results: residual scratches are gone and three operators now rate A02B00 porosity with 100% agreement. Eta phase shows crisp boundaries after 10% potassium ferricyanide etch, matching cross-section hardness mapping. Preparation time fell to 45 minutes per batch and the annual customer audit closed with zero findings.