Essentials of GB/T 228.1 Tensile Testing: Specimen, Rate Control and Yield Determination
Gauge length L₀=5.65√S₀, stress rate 2-60 MPa/s before yield; read ReH/R…
試験方法 · 測定原理

Gauge length L₀=5.65√S₀, stress rate 2-60 MPa/s before yield; read ReH/R…

E uses a step gauge over 5 lengths × 7 positions × 3 runs, P uses a refe…

2.5D adds Z via focus or laser for step heights; true 3D needs tactile p…

Edge points must localize to 1/10-1/50 pixel for repeatability below 0.3…

Even telecentric lenses keep some distortion; after full-field fitting w…

Resolution δ=0.61λ/NA rises with NA, but depth of field shrinks as 1/NA²…

A Nomarski prism shears the beam in two; nanometre surface steps become …

Sulfides, aluminates, silicates and globular oxides each split into fine…

The metallographic method counts structure, the hardness method counts t…

The comparison method is fast but uncertain to half a grade; the interce…

If the X and Y axes of a dual-axis instrument are not orthogonal, crosst…

A 0.1 °C gradient over a 1 m path deflects the beam by about 0.02″, and …