Nuclear materials2024

In-situ indentation creep of Zr-4 cladding at 400 °C, before and after irradiation

IMAS-HT700CM records 2-hour constant-load creep compliance with 12 points per specimen and drift within 0.4 µm, replacing multi-specimen uniaxial creep campaigns.

会社名
Materials institute of a nuclear research group
所在地
Chengdu, Sichuan
In-situ indentation creep of Zr-4 cladding at 400 °C, before and after irradiation
500 h → 4 hCampaign time
≤0.4 μmDrift (2 h)
-80%Specimen use

Zirconium cladding operates at 300–400 °C, where creep governs fuel-rod integrity. The institute previously used uniaxial creep frames: one specimen gave one stress level and needed more than 500 h, while irradiated specimens are extremely scarce.

Solution: instrumented indentation on IMAS-HT700CM at 400 °C under argon, 5 N held for 7200 s, depth versus time recorded and converted to an equivalent stress exponent using Oliver-Pharr and creep-compliance models; six indents per specimen.

Result: 12 data points per specimen, drift within 0.4 µm over 2 h; creep compliance rose 22% after irradiation, consistent with published neutron data; campaign time fell from 500 h to 4 h and specimen consumption by 80%.

⇄0比較仕様比較