Energy (wind power)2024

Low-temperature Charpy impact testing of wind-turbine bolts

JBS-300Z/500Z automatic impact tester with CDW-60 low-temperature bath runs Charpy V-notch tests at -40 ℃ to GB/T 229, specimen struck within 5 s of leaving the bath, bath fluctuation ±0.5 ℃.

会社名
A wind-power components plant, N. China
所在地
Zhangjiakou, Hebei
カテゴリ
Testing Machines
Low-temperature Charpy impact testing of wind-turbine bolts
39 JMean KV2 at -40 ℃
±0.5 ℃Bath fluctuation

Wind-tower high-strength bolts must reach KV2 of at least 27 J at -40 ℃. The manual pendulum with a dry-ice bath gave uneven temperatures, specimens warmed quickly after removal, and three-piece sets often spread more than 10 J, which the owner rejected.

Solution: a JBS-300Z/500Z automatic pendulum impact tester with 300/500 J dual ranges and automatic specimen feeding, plus a CDW-60 cascade-compressor bath holding -40 ℃ within ±0.5 ℃. The specimen travels from bath to strike within 5 seconds, meeting GB/T 229.

Result: 10.9-grade bolts measured 38, 41 and 39 J KV2 at -40 ℃, a 3 J spread; the tester passed verification to GB/T 3808.

Benefit: the low-temperature impact data were accepted by the owner at first submission, and bolt-lot release time was cut in half.

⇄0比較仕様比較