Automotive2024

In-line pull-out force testing of tie-rod ball pins

AGS-X13 benchtop electronic machine tests ball-pin pull-out force, 50 kN class 0.5, 40 seconds per piece, with full force-displacement curves kept for OEM traceability.

Company
An automotive steering systems plant, E. China
Address
Shanghai
In-line pull-out force testing of tie-rod ball pins
40 sTime per piece
36~42 kNPull-out force

After press-fitting, the tie-rod ball pin must demonstrate a pull-out force of at least 30 kN. The simple hydraulic puller only showed the peak value, hiding press-fit disturbances, and the OEM PPAP demanded process curves.

Solution: an AGS-X13 benchtop electronic universal testing machine, 50 kN class 0.5, with a dedicated ball-pin pull-out fixture. The program pulls at 10 mm/min, records the full force-displacement curve, and judges peak and yield knee automatically with archiving.

Result: 40 seconds per piece with pull-out forces of 36-42 kN; one double-peak curve anomaly was traced to press hydraulic-pressure fluctuation, keeping 2000 suspect parts from shipping.

Benefit: curve traceability satisfied the OEM PPAP requirement, and the line moved smoothly from pilot build to mass production.

⇄0CompareProduct comparison