Ô tô2024

Đo lực rút chốt cầu ro-tuyn lái

AGS-X13 50 kN đo lực rút chốt trong 40 giây, lưu toàn bộ đường cong.

Công ty
Nhà máy hệ thống lái ô tô, Đông Trung Quốc
Địa chỉ
Thượng Hải
Đo lực rút chốt cầu ro-tuyn lái
40 sThời gian/chi tiết
36~42 kNLực rút

After press-fitting, the tie-rod ball pin must demonstrate a pull-out force of at least 30 kN. The simple hydraulic puller only showed the peak value, hiding press-fit disturbances, and the OEM PPAP demanded process curves.

Solution: an AGS-X13 benchtop electronic universal testing machine, 50 kN class 0.5, with a dedicated ball-pin pull-out fixture. The program pulls at 10 mm/min, records the full force-displacement curve, and judges peak and yield knee automatically with archiving.

Result: 40 seconds per piece with pull-out forces of 36-42 kN; one double-peak curve anomaly was traced to press hydraulic-pressure fluctuation, keeping 2000 suspect parts from shipping.

Benefit: curve traceability satisfied the OEM PPAP requirement, and the line moved smoothly from pilot build to mass production.

⇄0So sánhSo sánh thông số