TY-9620 Photoelectric direct-reading OES spectrometer

Rapid quantitative elemental analysis

ModellTY-9620
  • Control火花放电直读(OES)
  • Measuring range金属全元素快速定量分析
  • Software工厂标准化曲线,牌号分选与成分报告
  • Power supplyAC 220 V

By submitting you agree to our privacy policy.

01

Überblick

The TY-9620 delivers rapid quantitative elemental analysis for metals and solutions in melt control, incoming and final inspection.

The TY-9620 delivers rapid quantitative elemental analysis for metals and solutions in melt control, incoming and final inspection.

02

Technische Daten

Control火花放电直读(OES)
Measuring range金属全元素快速定量分析
Software工厂标准化曲线,牌号分选与成分报告
Power supplyAC 220 V

* Generated by rule engine over the product database; for pre-selection only.

03

Messprinzip

Spark OES: a high-voltage spark in argon excites the metal surface; a grating disperses the emission lines onto CCD/PMT arrays, and calibration curves convert intensities into concentrations — 20–30 elements in 10–30 s, ideal for melt control and incoming checks.

ICP-OES: solutions nebulise into an argon plasma (6000–10000 K) for complete atomisation, enabling ppb-level multi-element analysis.

UV-Vis: Beer-Lambert law A = εbc with double-beam referencing for stable baselines (e.g. 7600S).

Flame photometry: alkali metals emit characteristic light in the flame with intensity proportional to concentration — simple and economical for K/Na/Li.

04

Process animation

  1. Sample: grind the metal face clean on a dedicated grinding disc.
  2. Purge: flood the stand with argon per procedure.
  3. Burn: pre-burn then analysis sparks.
  4. Read: line intensities collected by CCD/PMT.
  5. Quantify: calibration curves with type-standardisation give concentrations.
  6. Report: automatic grade judgement versus specification ranges.
0102030405
05

Calculation & formulas

1. Beer-Lambert: A = εbc; with ε=2000 L/(mol·cm), c=2×10⁻⁵ mol/L, b=1 cm, A = 0.040; keep absorbance between 0.1 and 0.8.

2. Calibration: ≥5 points with r² ≥ 0.999; run a mid-check each batch and recalibrate on >5% drift.

3. Detection limit: MDL = 3σ/slope; σ=0.002 Abs and slope 0.05 Abs/(mg/L) give 0.12 mg/L.

4. Type standardisation (OES): correct drift per element ki = Rref/Rmeas with a control sample at the start of each shift.

5. Internal standard: ratio R = Ielement/Imatrix cancels excitation fluctuations.

06

Normen

StandardTitleScope
GB/T 4336-2016Carbon and low-alloy steels by spark OESSteel quick analysis
GB/T 11170-2008Stainless steel by spark-discharge OESGrade judgement
GB/T 20975 seriesAluminium alloys by OESNon-ferrous metals
GB/T 9721-2006Chemical reagents — UV spectrophotometryUV-Vis quantitation
ISO 11885Water quality — ICP-OES for selected elementsEnvironmental ICP

Melt-control programs need per-grade control samples each shift; note spark conditions for interstitial elements.

07

Auswahl

1. Principle follows element and concentration: major and minor elements (0.001–30%) in metal use spark OES; trace levels (ppb to ppm) use ICP; single-element rapid quantification uses spectrophotometry or flame photometry.

2. Three things about OES: channel count and element coverage, detection limits (C/S/P are hardest), argon flush and standardisation. TY-9000 class suits multi-base steel and non-ferrous; Q4/Q8 suit high accuracy and precious metals.

3. Preparation decides data quality: flat, oxide-free, oil-free surfaces with a cutter and grinder; solid standards must match the matrix or matrix effects bias results by more than 10%.

4. ICP does not replace OES: OES is fast (90 s) on solid metal; ICP is slow (2 h preparation) on liquids and traces. Use OES for incoming metal, ICP for water.

5. Spectrophotometer by wavelength: visible (325–1000 nm) for routine colorimetry, UV-Vis (190–1100 nm) for organics and low concentrations, flame photometry for Na/K/Li/Ca.

6. Site and consumables: OES needs 99.999% argon, stable power and a dedicated earth; ICP needs a fume hood and argon; spectrophotometers need dark, stable temperatures.

ModelPrincipleStrengthTypical use
TY-9000 / TY-9610Spark OESMulti-element in steel and non-ferrousFurnace analysis, incoming checks
Q2 / Q4Spark OESMajor elements in metalsFoundries, machining
Q6 / Q8High-accuracy OESTrace C/S/P, precious metalsSpecial steel, precious metals
ICPE-9000 / ICPS-7510ICP-OESppb–ppm multi-elementWater, soil, food
UV1800UV-VisOrganic and inorganic colorimetryChemical, pharma, environment
7600SVisibleRoutine colorimetryTeaching, routine testing
FP640 / FP6410 / 6400AFlame photometryNa/K/Li/CaSoil, fertiliser, cement

What keeps data trustworthy: type standardisation with high and low standards every shift, full standardisation monthly, and matrix-matched standards.

08

Prüfverfahren

Metals: prepare a flat face by lathe or spectral grinder; specimens ≥3 mm thick and ≥φ20 mm, cooled before sparking.

Burn: 5–10 s flush plus 10–20 s analysis; ≥3 burns averaged, RSD >3% triggers investigation (gas, surface, segregation).

Calibration: one- or two-point type standardisation each shift; weekly full-curve checks; retain certificates.

UV-Vis: matched cells (≤0.5%), blank zeroing, absorbance 0.1–0.8.

ICP: complete digestion, on-line internal standard, matrix-matched standards, dilute high-salt samples to protect the nebuliser.

09

Industry applications

  • Steel and metallurgy: 90-second furnace analysis of C/Si/Mn/P/S/Cr/Ni/Mo to steer blowing and alloying; grade confirmation on finished product.
  • Non-ferrous: Si/Cu/Mg/Fe in aluminium, plus copper, zinc and titanium alloys to prevent grade mix-ups.
  • Foundries: per-heat spectrometry with retained samples, linking heat, composition and mechanical results.
  • Incoming material: grade verification against 304 substituted for 316 or 45 steel for 40Cr.
  • Environment and water: heavy metals (Cr/Ni/Cu/Zn/Pb/Cd), COD and ammonia in plating effluent and surface water by ICP and spectrophotometry.
  • Food and agriculture: heavy metals in grain, available phosphorus and potassium in soil, fertiliser nutrients by flame photometry and spectrophotometry.
  • Chemical and pharma: raw-material purity and reaction monitoring by UV-Vis and chromatography.
  • Precious metals: gold, silver and platinum-group content with high-precision OES or XRF.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0VergleichTechnischer Vergleich