FP640 Flame photometer

Rapid quantitative elemental analysis

ModellFP640
  • Control火焰发射法
  • Measuring rangeK / Na / Li / Ca / Ba 等元素快速测定
  • Power supplyAC 220 V

By submitting you agree to our privacy policy.

01

Überblick

The FP640 delivers rapid quantitative elemental analysis for metals and solutions in melt control, incoming and final inspection.

The FP640 delivers rapid quantitative elemental analysis for metals and solutions in melt control, incoming and final inspection.

02

Technische Daten

Control火焰发射法
Measuring rangeK / Na / Li / Ca / Ba 等元素快速测定
Power supplyAC 220 V

* Generated by rule engine over the product database; for pre-selection only.

03

Messprinzip

Spark OES: a high-voltage spark in argon excites the metal surface; a grating disperses the emission lines onto CCD/PMT arrays, and calibration curves convert intensities into concentrations — 20–30 elements in 10–30 s, ideal for melt control and incoming checks.

ICP-OES: solutions nebulise into an argon plasma (6000–10000 K) for complete atomisation, enabling ppb-level multi-element analysis.

UV-Vis: Beer-Lambert law A = εbc with double-beam referencing for stable baselines (e.g. 7600S).

Flame photometry: alkali metals emit characteristic light in the flame with intensity proportional to concentration — simple and economical for K/Na/Li.

04

Process animation

  1. Sample: grind the metal face clean on a dedicated grinding disc.
  2. Purge: flood the stand with argon per procedure.
  3. Burn: pre-burn then analysis sparks.
  4. Read: line intensities collected by CCD/PMT.
  5. Quantify: calibration curves with type-standardisation give concentrations.
  6. Report: automatic grade judgement versus specification ranges.
0102030405
05

Calculation & formulas

1. Beer-Lambert: A = εbc; with ε=2000 L/(mol·cm), c=2×10⁻⁵ mol/L, b=1 cm, A = 0.040; keep absorbance between 0.1 and 0.8.

2. Calibration: ≥5 points with r² ≥ 0.999; run a mid-check each batch and recalibrate on >5% drift.

3. Detection limit: MDL = 3σ/slope; σ=0.002 Abs and slope 0.05 Abs/(mg/L) give 0.12 mg/L.

4. Type standardisation (OES): correct drift per element ki = Rref/Rmeas with a control sample at the start of each shift.

5. Internal standard: ratio R = Ielement/Imatrix cancels excitation fluctuations.

06

Normen

StandardTitleScope
GB/T 4336-2016Carbon and low-alloy steels by spark OESSteel quick analysis
GB/T 11170-2008Stainless steel by spark-discharge OESGrade judgement
GB/T 20975 seriesAluminium alloys by OESNon-ferrous metals
GB/T 9721-2006Chemical reagents — UV spectrophotometryUV-Vis quantitation
ISO 11885Water quality — ICP-OES for selected elementsEnvironmental ICP

Melt-control programs need per-grade control samples each shift; note spark conditions for interstitial elements.

07

Auswahl

1. Principle follows element and concentration: major and minor elements (0.001–30%) in metal use spark OES; trace levels (ppb to ppm) use ICP; single-element rapid quantification uses spectrophotometry or flame photometry.

2. Three things about OES: channel count and element coverage, detection limits (C/S/P are hardest), argon flush and standardisation. TY-9000 class suits multi-base steel and non-ferrous; Q4/Q8 suit high accuracy and precious metals.

3. Preparation decides data quality: flat, oxide-free, oil-free surfaces with a cutter and grinder; solid standards must match the matrix or matrix effects bias results by more than 10%.

4. ICP does not replace OES: OES is fast (90 s) on solid metal; ICP is slow (2 h preparation) on liquids and traces. Use OES for incoming metal, ICP for water.

5. Spectrophotometer by wavelength: visible (325–1000 nm) for routine colorimetry, UV-Vis (190–1100 nm) for organics and low concentrations, flame photometry for Na/K/Li/Ca.

6. Site and consumables: OES needs 99.999% argon, stable power and a dedicated earth; ICP needs a fume hood and argon; spectrophotometers need dark, stable temperatures.

ModelPrincipleStrengthTypical use
TY-9000 / TY-9610Spark OESMulti-element in steel and non-ferrousFurnace analysis, incoming checks
Q2 / Q4Spark OESMajor elements in metalsFoundries, machining
Q6 / Q8High-accuracy OESTrace C/S/P, precious metalsSpecial steel, precious metals
ICPE-9000 / ICPS-7510ICP-OESppb–ppm multi-elementWater, soil, food
UV1800UV-VisOrganic and inorganic colorimetryChemical, pharma, environment
7600SVisibleRoutine colorimetryTeaching, routine testing
FP640 / FP6410 / 6400AFlame photometryNa/K/Li/CaSoil, fertiliser, cement

What keeps data trustworthy: type standardisation with high and low standards every shift, full standardisation monthly, and matrix-matched standards.

08

Prüfverfahren

Metals: prepare a flat face by lathe or spectral grinder; specimens ≥3 mm thick and ≥φ20 mm, cooled before sparking.

Burn: 5–10 s flush plus 10–20 s analysis; ≥3 burns averaged, RSD >3% triggers investigation (gas, surface, segregation).

Calibration: one- or two-point type standardisation each shift; weekly full-curve checks; retain certificates.

UV-Vis: matched cells (≤0.5%), blank zeroing, absorbance 0.1–0.8.

ICP: complete digestion, on-line internal standard, matrix-matched standards, dilute high-salt samples to protect the nebuliser.

09

Industry applications

  • Steel and metallurgy: 90-second furnace analysis of C/Si/Mn/P/S/Cr/Ni/Mo to steer blowing and alloying; grade confirmation on finished product.
  • Non-ferrous: Si/Cu/Mg/Fe in aluminium, plus copper, zinc and titanium alloys to prevent grade mix-ups.
  • Foundries: per-heat spectrometry with retained samples, linking heat, composition and mechanical results.
  • Incoming material: grade verification against 304 substituted for 316 or 45 steel for 40Cr.
  • Environment and water: heavy metals (Cr/Ni/Cu/Zn/Pb/Cd), COD and ammonia in plating effluent and surface water by ICP and spectrophotometry.
  • Food and agriculture: heavy metals in grain, available phosphorus and potassium in soil, fertiliser nutrients by flame photometry and spectrophotometry.
  • Chemical and pharma: raw-material purity and reaction monitoring by UV-Vis and chromatography.
  • Precious metals: gold, silver and platinum-group content with high-precision OES or XRF.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0VergleichTechnischer Vergleich