Automotive2022

Tensile strength and elongation testing of seatbelt webbing

WDW10-100 electronic machine tests seatbelt webbing breaking strength and elongation to GB 14166; wrap-type pneumatic grips stop slippage, cutting grip-break rate from 30% to zero.

Firma
An automotive webbing plant, E. China
Adresse
Nantong, Jiangsu
Tensile strength and elongation testing of seatbelt webbing
30% → 0Grip-break rate
28.6~30.2 kNBreaking strength

Seatbelt webbing must reach a breaking strength of at least 26 kN. The old flat-push grips let the webbing slip, specimens often broke at the jaws and were voided, and supplier and OEM data never matched.

Solution: a WDW10-100 computer-controlled electronic universal testing machine, 100 kN class 0.5, with wrap-type pneumatic grips lined with emery cloth. Testing follows GB 14166 at 100 mm/min, recording breaking strength and elongation automatically.

Result: breaking strength measured 28.6-30.2 kN with elongation of 11.5%; the grip-break rate fell from 30% to zero, and comparison with the OEM agreed within 1.5%.

Benefit: supplier and OEM data are now mutually recognised, eliminating about 120 repeated tests per month.

⇄0VergleichTechnischer Vergleich