Nuclear materials2024

72-hour in-situ hold indentation of cladding at 1200 °C

IMAS-HT1300CM logged 72-hour force-displacement curves and separated secondary creep rates, replacing 80% of conventional creep specimens.

Firma
Nuclear-materials laboratory, SW China
Adresse
Chengdu, Sichuan
72-hour in-situ hold indentation of cladding at 1200 °C
72 hLongest hold
80%Frame time saved

Creep evaluation of zirconium and candidate cladding alloys relied on banks of creep frames taking weeks per dataset.

Solution: IMAS-HT1300CM at 1200 °C stepped to 2 kgf and held for 72 h with 0.01% FS displacement resolution, three indent sites per temperature point under high-purity argon.

Result: secondary creep rates correlated at 0.95 with conventional specimens; per-point turnaround fell from three weeks to three days, saving 80% of screening frame time, with in-situ imaging confirming no recrystallisation artefacts.