Metrology and testing2024

Interlaboratory comparison of Vickers hardness at 1200℃

HMAS-HT1200 served as the pilot instrument in a 6-lab 1200℃ Vickers comparison; all En values were below 1.

Firma
A provincial metrology institute, E. China
Adresse
Zhejiang
Interlaboratory comparison of Vickers hardness at 1200℃
6Participating labs
< 1En value

The institute organized the first national 1200℃ interlaboratory comparison of Vickers hardness and needed a pilot instrument with proven long-term repeatability plus homogeneous transfer blocks.

Solution: HMAS-HT1200 verified the homogeneity of nickel-alloy transfer blocks at 1200℃ (10-indext HV10 range ≤2.5%); the comparison followed JJG 112 and ISO 6507-2 with 10 kgf load, 15 s dwell, and argon protection.

Result: all six participating labs stayed within ±4% of the reference value with En < 1. The report now underpins the national traceability chain for hot hardness.

⇄0VergleichTechnischer Vergleich