Tensile modulus of CFRP laminates with a video extensometer

WDS-100G with a video extensometer cuts modulus scatter from ±6% to ±1.8% and avoids knife-edge damage on the specimen.

Firma
Carbon-fibre products company, Jiangsu
Adresse
Changzhou, Jiangsu
Tensile modulus of CFRP laminates with a video extensometer
±6% → ±1.8%Modulus scatter
0.5 μmStrain resolution
无Specimen damage

Clip-on extensometers left knife-edge marks on CFRP and slipped, so strain readings jumped and modulus scatter across five specimens reached ±6%, making it impossible to separate material variation from measurement error.

Solution: WDS-100G electromechanical frame (100 kN, ±0.5% speed accuracy) with a video extensometer using target marks at 0.5 µm resolution; loaded at 2 mm/min per ASTM D3039 with modulus fitted between 0.1% and 0.3% strain.

Result: modulus repeatability ±1.8% with undamaged specimens available for fractography; a 4% difference between two batches traced to fibre volume fraction in the prepreg, tightening incoming inspection.