Cracks in C/C brake blanks closed after cooling, so the lab could not distinguish real interface damage between 1400℃ and 1600℃ service conditions.
Solution: IMAS-UHT1700CM applied 500 gf indents at 1600℃ under 10-3 Pa vacuum, with a 10X objective recording fiber-bundle debonding and matrix fragmentation at temperature; 6 indents per point at 1200/1400/1600℃.
Result: the debond-length-to-diagonal ratio was 2.8 at 1600℃ versus 1.6 at 1200℃. The hot damage criterion derived from this ratio correlates with rig wear at R2=0.89.