Automotive body-in-white2024

Shear and cross-tension testing of spot welds

Dedicated fixtures on a 500 kN frame evaluate nugget diameter and failure mode to ISO 14273/14272.

Firma
Joint-venture OEM, Hubei
Adresse
Wuhan, Hubei
Shear and cross-tension testing of spot welds
2%Eccentricity
-22%Spatter rate

Spot welds in high-strength steel need shear and cross-tension strength data. The previous small frame lacked fixture stiffness, caused eccentric loading and made failure-mode reading unreliable.

Solution: WAW-500C with self-aligning shear and cross-tension fixtures, tested at 10 mm/min to ISO 14273 and ISO 14272. The software logs peak force, displacement and curve shape to distinguish interfacial from base-metal failure.

Result: eccentricity reduced from 8% to 2%, 95% agreement in failure-mode classification, 60 test sets per shift, and data feeding the weld-parameter model cut spatter by 22%.