Chế tạo đắp dần2024

HXZDQ-100Z cắt chính xác mẫu titan in 3D

HXZDQ-100Z cắt chính xác mẫu SLM TC4 không cháy; độ rỗng 0,08% theo ảnh, thông lô nhanh gấp 3 lần.

Công ty
Trung tâm in 3D, Đông Trung Quốc
Địa chỉ
Thượng Hải
HXZDQ-100Z cắt chính xác mẫu titan in 3D
<5 μmLớp cháy cắt
0.08%Độ rỗng

SLM-built TC4 parts require porosity below 0.2%. Abrasive cut-off sampling caused a 50 um heat-tinted layer that rounded pore edges, so image analysis read 30% low and release depended on destructive tensile sampling.

Solution: an HXZDQ-100Z precision metallographic cutter with a low-speed 300 rpm diamond blade and full immersion cooling keeps the burn layer under 5 um. Vacuum-impregnated epoxy cold mounting avoids pore-fill artefacts, and polishing finishes with 0.05 um diamond suspension.

Results: on unetched polished sections, 20-field image analysis reads a stable 0.08% porosity, within 0.01 percentage points of X-ray CT. Lot release switched from tensile sampling to metallography, cutting release time from 5 days to 1.5 days.