Твёрдые сплавы2023

Определение зерна WC методом интерцептов

HMM-200: зерно WC 0,4 мкм по GB/T 3488, повторяемость ±0,03 мкм.

Компания
Завод твёрдых сплавов, Центр. Китай
Адрес
Хунань
Категория
Микроскопы
Определение зерна WC методом интерцептов
±0.03 μmПовторяемость

Developing a 0.4 μm ultrafine grade, the plant outsourced grain sizing to SEM labs with a one-week turnaround, too slow for lot release.

Solution: the HMM-200 microscope with a 100X/1.25 high-NA objective applies the GB/T 3488 intercept method at 1500X, 3 fields per sample and no fewer than 100 intercepts per field, with automatic image analysis.

Result: measured grain size was 0.38-0.42 μm, within 5% of SEM, with ±0.03 μm repeatability. Lot release went from 7 days to same-day, saving about RMB 400,000 in annual testing fees.

⇄0СравнениеСравнение характеристик